When a MIM part has been tested successfully. Normally when you set all the paremeters to go along with mass production, please do take the volume of nitric acid and time during debinding. Especially when the part is big, we suggest to add acid a bit and make the debinding time longer a bit. The following picture is a big part that is not debinded fully100% and lead to craks